Besides these printer settings for ALLPHA,
Adviced 3D printing temperature 190-200C* |
Adviced 3d print speed 40 - 80 mm/s |
Advised Heated bed |
Cooling fan 100% cooling. |
We also advise:
1 Fan Speed
The fan speed needs to be on full speed as soon as possible. How soon you can activate 100% coolinf fan may depend on your printer, but in general the sooner the better. We want to remove heat from the material as soon as possible to stop crystallization process.
2 Brim
We recommend using a brim for better adhesion of corners which might lift due to internal shrinkage. We generally use 20 perimeter for a brim.
3 Retraction settings
On most 3D printers the retraction settings can be set a bit lower then you would for PLA. If you see small gaps in the outside surface of the print it might be a sign the retract values are set just a bit too high.